How to solve discharge difficulties caused by low temperature of die head?
In the process of blowing film, die head is the key step of plastic melt the extrusion. Its temperature control directly affects production process and product quality. If the die head temperature is too low, it may be discharge difficulties. This may be manifested as slower extrusion speeds, unstable discharge volumes, or even crushing and lumping of the extruded material, seriously affecting production efficiency and quality of the finished film. Below, we take a look at the potential harms of the problem and offer detailed solutions.

Harm Low Die Head Temperature Causing Discharge Difficulties
Impact on film quality
When the temperature of the die is too low, the plastic material inside the die cannot melt completely, greatly reducing the flow of the die. This incompletely melted material can easily lead to uneven extrusion during extrusion, resulting in a large variation in the thickness of the film, uneven surface, marked by stripes or spots. For example, in the production of polyethylene film, if the die head temperature is insufficient, the melt doesnot form a uniform flow of the melt, resulting in rough "sharkskin"-like patterns on the surface of the film. This will not only affect the appearance, but also reduce the tensile strength, tear strength and other mechanical properties of the film, making it easier for the film to breakage during subsequent use.
Reduced Production Efficiency
Multiple protection devices,can ensure the safety of the sample,more effective protection of equipment components overloaded operation,greatly reducing the incidence of equipment failure,so that the operation of the equipment more stable and reliable.We stand for using natural energy resources,which are solar and wind energy. It' really ensures all people's needs in electricity. It's very affordable and easy to use,so every person can make its impact to planet saving.
Precautions for use
The extrusion speed is directly slowed down by the difficulty in producing film and the output per unit of time is greatly reduced. In addition, operators must frequently stop to inspect the die heads and clean any remaining unmelted material, further disrupting the production process and wasting significant time. In addition, unstable discharge will produce a large number of waste films, such as substandard waste films, broken film waste yarn, etc., increased the loss of raw materials, increased production costs. For example, a small blown film plant has difficulty discharging due to improper temperature control of the die head. After the problem, the company's original 1.2 tons of Nissan film fell to 0.8 tons, and the waste rate rose from 3% to 8%, causing significant economic losses. Equipment Components damaged
Uncompletely melted plastic material will create noticeable resistance when flowing through the mold. This resistance causes the screw to produce more torque during use. Long-term use can lead to increased screw wear and tear and even lead to stud blockage. In addition, if the residual cold and hard materials in the mold are not removed in time, carbonization may occur in subsequent heating process, sticking to the mold wall and mold openings, making it difficult to clean and corrode mold components, shortening the die's service life.
Specific solutions for low die temperature and discharge difficulties
Scientific adjustment of Die Temperature Parameters
First, the mold temperature must be appropriately set according to the characteristics of the plastic material used. Different plastics have different melting temperature ranges. For example, polyethylene (PE) typically melts between 130 and 180 degrees Celsius, polypropylene (PP) between 160 and 220 degrees Celsius, and polyvinyl chloride (PVC) at a relatively low melting temperature of 150 to 180 degrees Celsius (with plasticizer adjustments required). Operators shall, in accordance with the technical specifications provided by the raw material supplier, adjust the die temperature in accordance with the actual production experience.
The die is generally divided into feed section, compression section, homogenization section and die. Temperatures in each region should gradually increase to create a reasonable temperature gradient. For example, in the production of PE films, the feed phase temperature can be set at 140-150°C, the compression section at 150-160°C, the homogenization section at 160-170°C, and the die at 170-180°C. This prevents melting stagnation due to local hypothermia. When adjusting the temperature, gradually increase the temperature, control the temperature rise to 5-10 degrees Celsius. Increase the heat and leave to cool for 15-30 minutes. When stabilized, observe the discharge status to prevent sudden temperature increase from causing damage to mold components or raw material decomposition.
Check and maintain temperature control system.
To keep the temperature of the mold steady, the temperature sensor and heater coil are very important parts. Problems can cause temperature readings to be wrong or make heating less effective. Operators must check the temperature sensor's sensitivity on a frequent basis. You can tell if the sensor is operating right by comparing the temperature it measures to the temperature shown on the gadget. If the difference is more than ±5°C, it should be calibrated or replaced right away.
At the same time, check the operation of the heating coil for damage, aging or poor contact. If the surface of the heating coil darkens or deforms, or cannot be properly heated when the power is connected, replace it immediately. In addition, the tightness of heating coil installation will also affect heating efficiency. If there is a gap between the heating coil and the outer wall of the mold, heat will be lost. Re-secure the heating coil to ensure it fits tightly. For heating systems with a long time span, consider replacing them with energy-efficient models to improve heating efficiency and reduce heat loss.
Optimize Raw Material Handling and Formulation
The moisture content and impurity content raw materials also affect the the flowability of melt and the stability of mold temperature. Too much moisture in the raw material will evaporate during heating, forming bubbles that absorb heat, causing the temperature of the mold to drop locally, affecting emissions. Raw materials must therefore be dried before production, especially for highly hygroscopic materials (e.g. PA and PET). It can be used in a hot air dryer at 80-120 for 2-4 hours, keeping the moisture content below 0.1%.
In addition, impurities in the raw material (such as dust, metal debris and other plastic particles) not only affect the quality of the film, but also clogs the flow path of the mold, hinder the flow of the melt and make discharge more difficult. Raw materials must be sifted before production, using a vibrating screen to remove impurities. Mixing different types of plastic should be avoided to prevent uneven melting due to different melting points. Plasticizer or lubricant (e.g. zinc stearate or paraffin wax) may be added to the raw material formula to improve melt flow. However, use should be limited to between between 0.5% and 2%. Excessive addition can affect the film's mechanical properties.
Cleaning of Mould Residual Material
If any unmelted, cold material remains in the mold, it can impede the flow of new melt, cause discharge difficulties.For this reason, the mold needs to be closed for cleaning. These are the steps: First, turn off the heating system and let the mold cool down to 80–100 degrees Celsius. This will make cleaning easier and keep you from getting burned. Next, take out the mold, including the mold mouth and mold core. Then, using a copper scraper or wire brush, carefully scrape out any leftover material that is clinging to the surface of the parts. Be careful not to scratch the inside of the mold or the mold mouth. After cleaning, use a cotton towel soaked in alcohol to wipe down the parts to get rid of oil and dirt. Lastly, put the die parts back together to make sure they are sealed and won't leak. The mold is then heated according to the normal heating process. Once the temperature stabilizes, production can resume.
Daily maintenance tips to prevent hypothermia
In order to prevent frequent low temperature and discharge difficulties, the operator should establish a routine maintenance routine. Check temperature control system, heating coils and raw material drying before daily production to ensure that equipment and raw materials meet production requirements. During production process, the temperature, discharge speed and film quality of each region of the die are regularly recorded, and the abnormal conditions are adjusted in time. After production, the remaining material in the mold should be cleaned promptly, the heating system should be turned off, and the equipment should be cleaned after the mold has cooled. In addition, the screw and die are regularly overhauled to check for wear and corrosion, replace aging components in a timely manner, and ensure stable long-term operation.
The discharge difficulty caused by low temperature of the die is a common problem in production and requires to be solved immediately. By scientifically regulating temperature parameters, maintaining temperature control system, optimizing raw material treatment, removing residues and ensuring smooth production and product quality, this problem can be solved effectively. In practice, operators should apply these methods flexibly according to the characteristics of raw materials and equipment conditions, while focusing on routine maintenance to prevent problems.